学习与工作情况 2017.12-至今,西安理工大学 材料科学与工程学院,副教授 2014.12-2017.12,西安理工大学 材料科学与工程学院,讲师 2010.09-2014.12,西北工业大学,博士(硕博连读) 2008.09-2011.03,西北工业大学,硕士 2004.09-2008.07,西安工业大学,学士

研究领域

1. 合金凝固,包括定向凝固、普通凝固(感应熔炼、电弧熔炼等)、快速凝固等;2. 金属间化合物(NiAl)基共晶复合材料微观组织与力学性能等方面的研究;3. 粉末冶金;

近期论文

查看导师新发文章 (温馨提示:请注意重名现象,建议点开原文通过作者单位确认)

[1] Lei Wang*,et al., Stability of lamellar structure of directionally solidified NiAl-28Cr-6Mo eutectic alloy at different withdrawal rates and temperatures.Intermetallics 2018, 94: 83-91. [2]Lei Wang*,et al.,A true change of NiAl-Cr(Mo) eutectic lamellar structure during high temperature treatment.Journal of Alloys and Compounds 2018, 732: 124-128. [3]Lei Wang*,et al., Microstructure evolution and room temperature fracture toughness of as-cast and directionally solidified novel NiAl-Cr(Fe) alloy.Intermetallics 2017, 84: 11-19. [4]Lei Wang*,et al., Microstructure, fracture toughness and compressive property of as-cast and directionally solidified NiAl-based eutectic composite.Materials Science and Engineering A 2016, 664: 188-194. [5]Lei Wang*,et al., Effect of withdrawal rate on the microstructure and room temperature mechanical properties of directionally solidified NiAl-Cr(Mo)-(Hf, Dy)-4Fe alloy.Journal of Alloys and Compounds 2016, 663: 187-195. [6]Lei Wang*,et al., Effect of withdrawal rate and Gd on the microstructures of directionally solidified NiAl-Cr(Mo) hypereutectic alloy.Journal of the minerals, metals and materials society (JOM) 2016, 68: 1037-1045. [7]Lei Wang*,et al., Microstructure and mechanical properties of NiAl-based hypereutectic alloy obtained by liquid metal cooling and zone melted liquid metal cooling directional solidification techniques.Journal of Materials Research 2016, 31: 646-654. [8]Lei Wang*,et al., Effect of heat treatment on the microstructure and elevated temperature tensile property of Fe-doped NiAl-Cr(Mo)-(Hf,Dy) eutectic alloy.Materials Science and Engineering A 2016, 654: 177-183. [9]Lei Wang,et al., Microstructure evolution and enhancement of fracture toughness of NiAl-Cr(Mo)-(Hf,Dy) alloy with a small amount addition of Fe duringheat treatments.Scripta Materialia 2014, 89: 1-4 [10]Lei Wang,et al., Microstructure and mechanical property of directionally solidified NiAl–Cr(Mo)-(Hf, Dy) alloy at different withdrawal rates.Materials Science and Engineering A 2014, 607: 113-121 [11] Lei Wang,et al., Effect of Dy on the microstructures of directionally solidified NiAl-Cr(Mo) hypereutectic alloy at different withdrawal rates.Intermetallics 2014, 44: 44-54 [12] Lei Wang,et al., The effect of the flow driven by a travelling magnetic field on solidification structure of Sn-Cd peritectic alloys.Journal of Crystal Growth 2012, 356: 26-32 [13] Lei Wang,et al., Influences of travelling magnetic field on the dendritic structures of Sn–Cd peritectic alloy during directional solidification.Applied Physics A 2013, 112(2): 363-370 [14] Lei Wang,et al., Microstructure investigation of directionally solidified NiAl-Cr(Mo)-хDy (х= 0, 0.1 wt%) hypereutectic alloys at different withdrawal rates.Journal of the minerals, metals and materials society (JOM) 2013, 65(11): 1419-1425. [15] Lei Wang,et al., Effect of a travelling magnetic field on the interface morphology in directionally solidified Sn-Cd alloy.Transactions of Nonferrous Metals Society of China2013, 23(8): 2454-2459.

推荐链接
down
wechat
bug