个人简介
主要教育经历
2010-2009,日本东北大学金属材料研究所后藤研,访问留学
2007,3-2007,7 广州外语外贸大学国际留学部,英语培训
2003-1999,中南大学粉末冶金研究院,材料学博士
1999-1996,中南工业大学化学系,应用化学硕士
工作经历
1994-1997,湘潭市第二职业中学,任教
1999-至今,中南大学
研究领域
快速化学气相沉积,炭/炭复合制动材料、树脂基材料、高性能高温抗氧化涂层、医用生体材料等
近期论文
查看导师新发文章
(温馨提示:请注意重名现象,建议点开原文通过作者单位确认)
1).殷延雄,于澍,李云平,吴强,李晓等,炭基复合材料生物相容性研究,生物医学工程学杂志, 2018,35(5):740-748
2).Qiang Wu, Shu Yu, Hui Zhong, Xiao Li, et al. Preparation of silicon carbide coating by chemical vapor deposition by using hxamethyldisilylamine precursor, Surface & Coatings Technology, 2018,334:78-83
3).吴强,于澍,李云平等, C/C复合材料的非晶SiO2涂层制备及其生物活性[J].复合材料学报,2017(34)7:1582-1588;
4).Li X, Yu S, Li YP, et al. Effect of pre-fatigue on bending behavior of 2.5D C/C composites[J]. Materials Science & Engineering A, 2017, 682:290-295.
5).李晓,于澍,刘京等. 接骨板用材料的研究现状及发展前景[J]. 生物医学工程学杂志, 2016(6):1214-1219.
6).刘京,肖鹏,于澍等. 炭基复合材料与人骨的力学性能对比分析[J]. 复合材料学报,2016,33(11):2657-2665
7).Shu Yu,Rong Tu,Takashi Goto,Preparation of SiOC nanocomposite films by laser chemical vapor deposition,Journal of European Ceramic Society,2016,36(3):403-409
8).Shu Yu, Fuqing Zhang, Xiang Xiong, Tribological properties of carbon/carbon composites with various pyrolytic carbon microstructures, Wear, 304(2013):103–108
9).Yunping Li, Emi Onodera, Hiroaki Matsumoto, Yuichiro Koizumi, Shu Yu*, Akihiko Chiba, Development of Novel Methods for Compensation of Stress-strain Curves,ISIJ International, 2011,51(5):782-787
10).Shu Yu ,Zhoushun Zheng,Fuqing Zhang, Yongqiang Cai, Mathematical model for the precursor gas residence time in isothermal CVD process of C/C composites,Transactions of Nonferrous Materials Society of China, 2011,21(8):1833-1839
11).Shu Yu, Akihiko Ito, Rong Tu, Takashi Goto, Dome-like and dense SiC-SiO2 nanocomposite films synthesized by laser chemical vapor deposition using CO2 laser, Surface & Coatings Technology, 2011,205(8-9):2818-2822
12).Shu Yu, Rong Tu, Akihiko Ito, Takashi Goto, SiC-SiO2 nanocomposite films prepared by laser CVD using tetraethyl orthosilicate and acetylene as precursors,Materials Letters,2010,64(20):2151-2154
13).Shu Yu, Jie Chen, Qizhong Huang, Effect of braking speeds on the tribological properties of carbon/carbon composites, Materials Transactions, 2010,51(5):1038-1043
14).于澍,陈洁,黄启忠,以丙烯为炭源气的热解炭的制备及其沉积机理分析,材料导报,2010,24(12):53-55
15).于澍,陈洁,黄启忠,以丙烯为炭源气的化学气相沉积模型,炭素技术,2010,29(6):1-4
16).Guohui Wang, Shu Yu, Shaihong Zhu, Changqing Gao, Yong Liu, Yunliang Miu, Boyun Huang, Biological properties of carbon/carbon implant composites with unique manufacturing processes,J Mater Sci: Mater Med, 2009,20(12):2487-2492
17).于澍,黄伯云,熊翔,张传福,不同刹车压力下炭/炭复合材料的摩擦磨损性能,新型炭材料,2008,23(2):127-131
18).Yunping Li, Shu Yu, Thermal-mechanical process in producing high dispersed tungsten-copper composite powder,International Journal of Refractory Metals and Hard Materials,2008,26(6):540-548
19).于澍,张红波,张传福,廖寄乔, 邓艳梅,热解炭的表征,航空材料学报,2007,27(1):57-60