近期论文
查看导师新发文章
(温馨提示:请注意重名现象,建议点开原文通过作者单位确认)
[1] Guangming Zheng*, Xiang Cheng, Li Li, Rufeng Xu, Yebing Tian. Experimental investigation of cutting force, surface roughness and tool wear in high-speed dry milling of AISI 4340 steel. Journal of Mechanical Science and Technology, 2019, 33(1): 341-349 (SCI, EI收录)
[2] Guangming Zheng*, Guoyong Zhao, Xiang Cheng, Rufeng Xu, Jun Zhao, Huaqiang Zhang, Frictional and wear performance of TiAlN/TiN coated tool against high-strength steel, Ceramics International, 2018, 44(6): 6878-6885 (SCI, EI收录)
[3] Guangming Zheng*, Li Li, Zhiyong Li, Jun Gao, Zongwei Niu, Wear mechanisms of coated tools in high-speed hard turning of high strength steel, International Journal of Advanced Manufacturing Technology, 2018, 94(9-12): 4553-4563 (SCI, EI收录)
[4] Guangming Zheng*, Rufeng Xu, Xiang Cheng, Guoyong Zhao, Li Li, Jun Zhao, Effect of cutting parameters on wear behavior of coated tool and surface roughness in high-speed turning of 300M, Measurement 125 (2018) 99-108 (SCI, EI收录)
[5]郑光明*, 程 祥, 杨先海, 徐汝锋, 赵 军, Al2O3/TiCN涂层刀具的滑动磨损性能及切削性能研究, 摩擦学学报, 2018, 38(3): 356-363 (EI收录)
[6] Guangming Zheng*, Xiang Cheng, Xianhai Yang, Rufeng Xu, Jun Zhao, Guoyong Zhao, Self-organization wear characteristics of MTCVD-TiCN-Al2O3 coated tool against 300M steel, Ceramics International, 2017, 43(16): 13214-13223 (SCI, EI收录)
[7] 郑光明*, 程祥, 牛宗伟, 高军, 房友飞,涂层硬质合金刀具高速车削 300M刀具磨损机理研究 制造技术与机床, 2017, (10): 98-102
[8] Guangming Zheng*, Jun Zhao, Xiang Cheng, Rufeng Xu, Guoyong Zhao, Experimental investigation on sialon ceramic inserts for ultra-high-speed milling of Inconel 718. Materials and Manufacturing Processes, 2016, 31(5): 633-940 (SCI, EI收录)
[9]郑光明*, 赵军, 徐汝锋, 孟建兵, 陶瓷刀具材料断口形貌及裂纹扩展的分形特征. 功能材料, 2015, 46(21): 21133-21136, 21143 (EI收录)
[10] 郑光明*, 赵 军, 程 祥, 徐汝锋, 李 丽. 梯度微纳米复合陶瓷刀具材料的力学性能和微观结构. 中国有色金属学报, 2016, 26(4): 844-851 (EI收录)
[11] Guangming Zheng*, Jun Zhao, Xiang Cheng, Min Wang. Self-sharpening failure characteristic of a Si3N4 ceramic tool in high speed cutting of Inconel 718. Key Engineering Materials, 2016, 693: 1135-1142 (EI收录)
[12] Guangming Zheng*, Jun Zhao, Li Li, Xiang Cheng, Min Wang, A fractal analysis of the crack extension paths in a Si3N4 ceramic tool composite, International Journal of Refractory Metals and Hard Materials, 2015, 51: 160-168 (SCI, EI收录)
[13] Guangming Zheng*, Jun Zhao, Zhiyong Li, Xiang Cheng, Li Li, Fractal characterization of the friction forces of a graded ceramic tool material, International Journal of Advanced Manufacturing Technology, 2014, 74: 707-714 (SCI, EI收录
[14] 郑光明*,赵军,徐汝锋,程祥,赵国勇, 陶瓷刀具超高速铣削镍基高温合金刀具失效机理研究, 组合机床与自动化加工技术, 2014, (10): 127-130
[15] 郑光明*, 赵军, 程祥, 赵国勇, 高速车削TC11分形特征实验研究, 制造技术与机床, 2014, (8): 130-133
[16] Guangming Zheng, Jun Zhao*, Yonghui Zhou, Anhai Li, Xiaobin Cui, Xianhua Tian, Performance of graded nano-composite ceramic tools in ultra-high-speed milling of Inconel 718, International Journal of Advanced Manufacturing Technology, 2013, 67: 2799-2810 (SCI, EI收录)
[17] Guangming Zheng, Jun Zhao*, Anhai Li, Xiaobin Cui, Yonghui Zhou, Failure mechanisms of graded ceramic tool in ultra high speed dry milling of Inconel 718, International Journal of Precision Engineering and Manufacturing, 2013, 14(6): 943-949 (SCI收录)
[18] Guangming Zheng, Jun Zhao*, Chao Jia, Xianhua Tian, Yongwang Dong, Yonghui Zhou, Thermal shock and thermal fatigue resistance of Sialon-Si3N4 graded composite ceramic materials, International Journal of Refractory Metals and Hard Materials, 2012, 35: 55-61 (SCI, EI收录) [19] Guangming Zheng, Jun Zhao*, Yonghui Zhou, Friction and wear behaviors of Sialon–Si3N4 graded nano-composite ceramic materials in sliding wear tests and in cutting processes, Wear, 2012, 190-191: 41-50 (SCI, EI收录)
[20] Guangming Zheng*, Jun Zhao, Zhongjun Gao, Qingyuan Cao, Cutting performance and wear mechanisms of Sialon–Si3N4 graded nano-composite ceramic tools, International Journal of Advanced Manufacturing Technology, 2012, 58: 19-28 (SCI, EI收录)
[21] Guangming Zheng*, Jun Zhao, Yonghui Zhou, Zhongjun Gao, Xiaobin Cui, Anhai Li, Fabrication and characterization of Sialon-Si3N4 graded nano-composite ceramic tool materials, Composites Part B: Engineering, 2011, 42 (7): 1813-1820 (SCI, EI收录)
[22] 郑光明, 赵 军*, 周咏辉, 高中军, Sialon-Si3N4系梯度纳米复合陶瓷刀具材料的设计及制备, 硅酸盐学报, 2011, 39(5): 783-788 (EI收录)
[23] 郑光明*, 赵 军, 宋新玉, 崔晓斌, 陶瓷刀具切削镍基合金的三维数值模拟, 组合机床与自动化加工技术, 2010, (3): 4-6, 10
[24] 郑光明*, 赵 军, 王晓琴, 硬质合金刀具车削钛合金时切削力分形特征研究, 工具技术, 2010, 44(1): 23-25
[25] Guangming Zheng*, Jun Zhao, Xinyu Song, Xiang Cheng, A fractal analysis of cutting force in simulation and experiment, 12th Conference on Machining and Advanced Manufacturing Technology, CMAMT 2013, Xiamen, P.R. China, 2013.07.24-07.27 (EI收录)
[26] Guangming Zheng*, Jun Zhao, Yonghui Zhou, Zhongjun Gao, Preparation and characterization of Si3N4/TiCN composite ceramic tool material, 2010 International Conference on Advances in Materials and Manufacturing Processes, ICAMMP 2010, Shenzhen, P.R. China, 2010.11.06-11.08 (EI收录)
[27] Guangming Zheng*, Jun Zhao, Xinyu Song, Qingyuan Cao, Yueen Li, Ultra high speed turning of Inconel 718 with Sialon ceramic tools, 13th International Symposium on Advances in Abrasive Technology, ISAAT2010, Taipei, Taiwan, 2010.09.19-09.22 (EI收录)
[28] 郑光明, 赵军, 周咏辉, 高中军, 一种梯度纳米复合陶瓷刀具材料及其制备方法, 2013.09.11, 中国, ZL201010220319.7