构建“三明治”结构以获得可回收性和高截留率的高通量CA@HMSN@h-BN/PDA膜,用于高效处理染料废水
Colloids and Surfaces A: Physicochemical and Engineering Aspects ( IF 4.9 ) Pub Date : 2023-07-13 , DOI: 10.1016/j.colsurfa.2023.132023 Shuyi Shang , Guoqing Xiao , Chunlin Chen , Chunyan Chen , Ruili Li , Zhengwei Yang , Min Cao , Rui Zou , Yaling Tang
"点击查看英文标题和摘要"
更新日期:2023-07-13
Colloids and Surfaces A: Physicochemical and Engineering Aspects ( IF 4.9 ) Pub Date : 2023-07-13 , DOI: 10.1016/j.colsurfa.2023.132023 Shuyi Shang , Guoqing Xiao , Chunlin Chen , Chunyan Chen , Ruili Li , Zhengwei Yang , Min Cao , Rui Zou , Yaling Tang
对于纺织工业废水的处理,有必要开发一种能高效去除染料分子且不易污染的纳滤膜。通过将中空介孔二氧化硅纳米粒子(HMSN)支撑层和h-BN/PDA隔离层组装在醋酸纤维素(CA)膜上,获得了一种新型高通量“三明治”结构的CA@HMSN@h-BN/PDA膜。HMSN使用 ZIF-8 作为自我牺牲模板合成,以提供改善的渗透性。聚多巴胺(PDA)对六方氮化硼(h-BN)进行改性得到的h-BN/PDA使膜具有更高的亲水性、截留率和稳定性。该研究解决了膜分离的问题该工艺需要牺牲通量和可回收性以获得高废品率。CA@HMSN@h-BN/PDA膜具有超亲水性能(水接触角为22.5°)和高纯水通量(4419.4 L·m -2·h-1·bar-1)。同时,由于特殊的“三明治”结构,CA@HMSN@h-BN/PDA膜实现了较高的截留率(超过99.5%)。通过循环实验,CA@HMSN@h-BN/PDA膜表现出可回收性。更重要的是,CA@HMSN@h-BN/PDA膜在复杂环境中保持稳定的性能,例如极酸/碱性或无机盐干扰环境。因此CA@HMSN@h-BN/PDA膜具有未来废水处理的潜力