透明质酸乙烯酯水凝胶的飞秒激光双光子聚合实现 22 nm 分辨率
ACS Applied Materials & Interfaces ( IF 8.3 ) Pub Date : 2023-05-23 , DOI: 10.1021/acsami.3c04346 Qi Duan 1, 2 , Wei-Cai Zhang 1, 2 , Jie Liu 1 , Feng Jin 1 , Xian-Zi Dong 1 , Fan-Chun Bin 1, 2 , Patrick Steinbauer 3, 4 , Elise Zerobin 4 , Min Guo 1, 2 , Teng Li 1, 2 , Stefan Baudis 3, 4 , Mei-Ling Zheng 1
ACS Applied Materials & Interfaces ( IF 8.3 ) Pub Date : 2023-05-23 , DOI: 10.1021/acsami.3c04346 Qi Duan 1, 2 , Wei-Cai Zhang 1, 2 , Jie Liu 1 , Feng Jin 1 , Xian-Zi Dong 1 , Fan-Chun Bin 1, 2 , Patrick Steinbauer 3, 4 , Elise Zerobin 4 , Min Guo 1, 2 , Teng Li 1, 2 , Stefan Baudis 3, 4 , Mei-Ling Zheng 1
Affiliation
三维 (3D) 仿生水凝胶由于其出色的生物相容性优势,在组织工程中发挥了重要作用。在这里,已经研究了高精度 3D 水凝胶的双光子聚合 (TPP),使用透明质酸乙烯酯 (HAVE) 作为生物相容性水凝胶单体的前体,3,3'-(((1 E , 1' E )-(2-oxocycloptane-1,3-diylidene) bis(methanylylidene)) bis(4,1-phenylene)) bis(methylazanediyl))dipropanoate 作为水溶性引发剂,d l-二硫苏糖醇 (DTT) 作为点击化学交联剂。通过调整光刻胶的溶解度和配方,全面研究了 HAVE 前驱体的 TPP 特性。在 3.67 mW 的加工激光阈值下获得了 22 nm 的特征线宽度,并制造了 3D 水凝胶支架结构。此外,3D 水凝胶的杨氏模量平均值为 94 kPa,并且已经证明了细胞生物相容性。这项研究将为在组织工程和生物医学中实现具有高精度配置的 3D 水凝胶支架提供巨大的潜力。
"点击查看英文标题和摘要"
更新日期:2023-05-23
"点击查看英文标题和摘要"