激光-电化学减材-增材混合制造法制备多级微纳超双疏性表面的策略
Colloids and Surfaces A: Physicochemical and Engineering Aspects ( IF 4.9 ) Pub Date : 2023-01-10 , DOI: 10.1016/j.colsurfa.2023.130946 Yang Liu , Jinzhong Lu , Wei Xue , Zhaoyang Zhang , Hao Zhu , Kun Xu , Yucheng Wu , Bo Wang , Weining Lei
"点击查看英文标题和摘要"
更新日期:2023-01-10
Colloids and Surfaces A: Physicochemical and Engineering Aspects ( IF 4.9 ) Pub Date : 2023-01-10 , DOI: 10.1016/j.colsurfa.2023.130946 Yang Liu , Jinzhong Lu , Wei Xue , Zhaoyang Zhang , Hao Zhu , Kun Xu , Yucheng Wu , Bo Wang , Weining Lei
为了在铜表面实现超双疏性能,探索了一种通过激光-电化学减材-增材制造方法制备多级微纳米超双疏膜的新策略。为了测试用该方法制备的金属表面的性能,进行了多种测试实验。实验结果表明,水滴和油滴的接触角(CA)分别为161°±4°和151°±4°,而滚动的CA为2°和10°,表明制备的表面具有优异的超双疏性能. 通过不同温度下的润湿性测试,制备的样品在低温5℃时的表面疏水性比室温25℃时差。根据液滴弹跳测试,当激光扫描间隔等于激光光斑直径时,水滴在制备的样品表面经历了两次完整的弹跳过程,表明稳定的卡西态与多能级微纳结构有关。此外,本文制备的超双疏性表面具有完善的功能性和稳定性,为在汽车、航空航天和造船工业中的潜在应用提供了一种新方法。