Ainara Valverde 1 , Renato Gonçalves 2 , María M. Silva 2 , Stefan Wuttke 1, 3 , Arkaitz Fidalgo-Marijuan 1, 4 , Carlos M. Costa 2, 5 , José L. Vilas-Vilela 1, 6 , José M. Laza 6 , María I. Arriortua 1, 7 , Senentxu Lanceros-Méndez 1, 3 , Roberto Fernández de Luis 1
ACS Applied Energy Materials ( IF 5.4 ) Pub Date : 2020-11-10 , DOI: 10.1021/acsaem.0c02044
Ainara Valverde 1 , Renato Gonçalves 2 , María M. Silva 2 , Stefan Wuttke 1, 3 , Arkaitz Fidalgo-Marijuan 1, 4 , Carlos M. Costa 2, 5 , José L. Vilas-Vilela 1, 6 , José M. Laza 6 , María I. Arriortua 1, 7 , Senentxu Lanceros-Méndez 1, 3 , Roberto Fernández de Luis 1
Affiliation
![]() |
制备了用于锂离子电池(LIB)的聚偏二氟乙烯(PVDF)和基于MOF-808的隔膜,并在形态和热性能,电解质吸收,保持力和表面亲水特性方面进行了充分表征。评估了PVDF / MOF-808隔板对LIB电化学性能的影响。PVDF / MOF-808膜表现出清晰的多孔结构,具有相互连接的大孔到中孔的均匀分布。基于Zr的MOF纳米颗粒的加入会增加隔板的孔隙率和表面积,从而提高电解质的吸收率和离子电导率。最后,MOF-808填料的存在改善了液体电解质的保留能力,从而防止了高C速率循环时容量下降。确实,4个半电池显示PVDF / MOF-808膜在2C速率下的放电容量为68 mAh·.g –1,而纯PVDF则为0 mAh·g –1。PVDF / 10 wt%MOF-808样品显示出长期稳定的循环行为,库仑效率接近100%。因此,表明复合膜相对于用于锂离子电池应用的常规隔膜而言是一种改进,因为它们将聚合物的介孔结构和大孔结构与MOF的规则排列的微孔系统结合在一起,从而大大改善了电解质的亲和性。